First pages of report (AutoRecovered) final
First pages of report (AutoRecovered) final
Submitted by
OMKAR U. POPALGHAT (T2121261191606)
OMKAR G. AKHARE (T2121261191571)
UMESH B. PAWDE (T2121261191581)
PRATIK M. BAGUL(T2121261191612)
SHAILESH CHAVAN (T2121261191565)
Dr. N. G. Patil
Director
MIT
Chh. Sambhajinagar
DECLARATION
We hereby declare that this written submission presents our ideas in our own word. We
have adequately referred the original sources. we also declare that we have adhered all
the principles of honesty and integrity and have not misprinted or fabricated or falsified
our idea/data/fact/source in our submission. We understand that any violation of the
above will be cause for disciplinary action by the institute
.
We would like to express our gratitude towards our guide Dr. Suhel Hashmi at every
step in the study of this work, contributed with his valuable guidance and provided with
perfect solution for every problem that arise. We would like to express our sincere and
hearty thanks to our respected Dr. P. R. Awsarmal, HCED and Dr. N.G. Patil, Director
of MIT Chh. Sambhajinagar for their insightful comments during the work. Our thanks
go to all staff members of Civil Engineering Department, MIT who helped us in
completion of this work.
Sr Figure Page no
No
1 Metal Laser Cutting Machine 9
2 Cold formed channel section 10
3 Flat coupons 10
4 Universal Testing Machine 11
5 Test Conducting 12
6 Coupons Testing In UTM 13
7 Failed Flat Coupons 15
8 Failed Curved Coupon 15
Sr Table Page no
No
1 Co-ordinates of stress strain graph 14
2 Comparison between Flat and curved coupon 16