0% found this document useful (0 votes)
99 views2 pages

European Steel and Alloy Grades: X6Crnicus18-9-2 (1.4570)

Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
99 views2 pages

European Steel and Alloy Grades: X6Crnicus18-9-2 (1.4570)

Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 2

3/6/2014 X6CrNiCuS18-9-2 / 1.

4570 - steel equivalent, mechanical properties, chemical composition

EURO PEAN ST EEL AND ALLO Y


G RADES
st eelnumber . com

Steel Steel and cast iron Alloy Equivalent Russian


Home Search About us
numbers standards standards grades steels

YOU HERE: Steel numbers -> Number 1.45XX OR Steel and cast iron standards -> / EN 10088-3 / EN 10088-
1

X6CrNiCuS18-9-2 ( 1.4570 )

Grade : X6CrNiCuS18-9-2

Number: 1.4570

EN 10088 - 3 : 2005 Stainless steels. Technical delivery conditions for semi-finished products, bars,
Standard: rods, wire, sections and bright products of corrosion resisting steels for general purposes
EN 10088 - 1 : 2005 Stainless steels. List of stainless steels.

Density: 7.9 g/cm ³

Classification: Austenitic stainless steel

Equivalent grades: No information

Che m ic a l c om pos it ion % of gr a de X 6 Cr NiCuS 1 8 - 9 - 2 ( 1 .4 5 7 0 )


C Si Mn Ni P S Cr Mo N Cu

max 0.08 max 1 max 2 8 - 10 max 0.045 0.15 - 0.35 17 - 19 max 0.6 max 0.11 1.4 - 1.8

M e c ha nic a l pr ope r t ie s of gr a de X 6 Cr NiCuS 1 8 - 9 - 2 ( 1 .4 5 7 0 )

Rm - Tensile strength (MPa) (+A) 500-710

Rp0.2 0.2% proof strength (MPa) (+A) 185

A - Min. elongation at fracture (%) (+A) 35

Brinell hardness (HB): (+A) 215

P r ope r t ie s of gr a de X 6 Cr NiCuS 1 8 - 9 - 2 ( 1 .4 5 7 0 )
Resistance to intergranular corrosion: in the delivery condition - no; in the sensitized condition - no

M e c ha nic a l pr ope r t ie s
M e c ha nis c he Eige ns c ha f t e n
Ca r a c t e r is t ique s m e c a nique s
R eH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d�elasticite minimale
R m Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc
http://www.steelnumber.com/en/steel_composition_eu.php?name_id=267 1/2
3/6/2014 X6CrNiCuS18-9-2 / 1.4570 - steel equivalent, mechanical properties, chemical composition
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc

He a t t r e a t m e nt c ondit ions
+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated

Chemical composition of X6CrNiCuS18-9-2 (1.4570). Equivalent grades of X6CrNiCuS18-9-2 (1.4570). Standards of


X6CrNiCuS18-9-2 (1.4570).
Properties of X6CrNiCuS18-9-2 (1.4570). Hardness of X6CrNiCuS18-9-2 (1.4570). Strength of X6CrNiCuS18-9-2 (1.4570).
Elongation of X6CrNiCuS18-9-2 (1.4570).

© 2011- 2014 All rights reserved. The contents from this site may not be reproduced.
The entire risk as to use of these content is assumed by you the user

http://www.steelnumber.com/en/steel_composition_eu.php?name_id=267 2/2

You might also like