This document provides information on 070M20 normalised carbon steel according to British Standard BS 970-1:1972,1983. It is an unalloyed wrought steel with a carbon content between 0.16-0.24% and includes manganese between 0.5-0.9%. Mechanical properties listed include an ultimate tensile strength of 62.4 ksi, yield strength of 31.2 ksi and elongation of 21%. The steel is normally heat treated by normalizing at temperatures between 880-910 degrees C and is available in forms such as bar, forgings and wrought.

Uploaded by

zaafr
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
491 views2 pages

070Mxx Normalised Carbon Steel To BS 970 Pt1 - 1972,1983

This document provides information on 070M20 normalised carbon steel according to British Standard BS 970-1:1972,1983. It is an unalloyed wrought steel with a carbon content between 0.16-0.24% and includes manganese between 0.5-0.9%. Mechanical properties listed include an ultimate tensile strength of 62.4 ksi, yield strength of 31.2 ksi and elongation of 21%. The steel is normally heat treated by normalizing at temperatures between 880-910 degrees C and is available in forms such as bar, forgings and wrought.

Uploaded by

zaafr
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 2

Page 1 of 2

070M20 normalised carbon steel to BS 970


Pt1:1972,1983
General Information
General Information/Comparable Grades
BS 970-1

Comparables:
UK: En3A, En3C

Notes and Applications


Unalloyed steel wrought.

Alloy Type Unalloyed steel: wrought

Standards Body/Status
Country UK
Standards Body BSI
Status Superseded

Composition (common elements)


Base Element Fe (Iron)
C (Carbon) 0.16 - 0.24 %
Fe (Iron) 99 %
Mn (Manganese) 0.5 - 0.9 %
P (Phosphorus) 0 - 0.05 %
S (Sulphur) 0 - 0.05 %
Balance Fe (Iron)
Notes
Fe (Iron) content is not given by the specification. The value stated is a calculated balance.
Chemical Composition Notes
Note: Where specifically ordered, a lower content of S and P, with each element at 0.025% maximum, may be
supplied. This is recommended for certain nitriding steels and for tensile strength ranges of 1225 N/mm2 minimum and
greater. Other limits for S and P may be agreed between the purchaser and supplier and stated on the order.
Unless otherwise stated in the material specification, steel can be supplied with P and S in a controlled range. (Please
consult original document. Page 4 Section 1.7.2.2.).

Mechanical Properties
Ultimate Tensile Strength (UTS) 62.4 ksi
Yield Strength 31.2 ksi
Elongation 21 %
Gauge Length 5.65vSo
Hardness (Brinell) 126 - 179 HB
Mechanical Properties Notes
Properties above are for LRS 150mm.
Properties also available for LRS 250mm if required.
Brinell hardness properties are for guidance only.

Thermal Treatment
Heat Treatment
Normalising temperature: 880-910 degs C.

Available Forms
Available forms Bar, Forgings, Other, Wrought

Data compiled and maintained by World Metal Index (Metal section) and TWI (Consumables section), licensed for distribution by Granta Design Ltd.
Granta provides no warranty for the accuracy of this data.
Page 2 of 2
070M20 normalised carbon steel to BS 970
Pt1:1972,1983
Links
MaterialUniverse equivalent alloys
MaterialUniverse similar alloys
Source of Information
Suppliers

Data compiled and maintained by World Metal Index (Metal section) and TWI (Consumables section), licensed for distribution by Granta Design Ltd.
Granta provides no warranty for the accuracy of this data.

You might also like