3.6 Analysis of Members Under Flexure (Part V)
3.6 Analysis of Members Under Flexure (Part V)
Analysis of Partially Prestressed Section Analysis of Unbonded Post-tensioned Beam Analysis of Behaviour
reinforcement is provided in addition to the prestressing steel. When this reinforcement is considered in the flexural capacity, the section is termed as a partially prestressed section.
The reasons for using a partially prestressed section are as follows. 1) The section is economical. 2) The cambering is less compared to an equivalent section without conventional reinforcement. 3) The ductility is more in a partially prestressed section. 4) Any reversal of moments (for example, due to earthquake) is not detrimental as compared to an equivalent section without conventional reinforcement.
Analysis A partially prestressed section can be either rectangular or flanged. A section can be doubly reinforced with reinforcement near the compression face.
Here, the equations for a doubly reinforced rectangular section are given. The following sketch shows the beam cross section, strain profile, stress diagram and force couples at the ultimate state.
b dp As Ap As d d
0.0035 s
0.447fck
xu fs
fs fpu
0.42xu
Cs Cc Tp Ts
Force
p
pu
Cross-section
Figure 3-6.1
Strain
Stress
The variables in the above figure are explained. b d d dp As As Ap = breadth of the section = depth of the centroid of the reinforcing steel (tension side) = depth of the centroid of the reinforcing steel (compression side) = depth of the centroid of prestressing steel (CGS) = area of the reinforcing steel (tension side) = area of the reinforcing steel (compression side) = area of the prestressing steel = strain difference in the prestressing steel when strain in concrete is zero = depth of the neutral axis at ultimate = strain in reinforcing steel (tension side) at ultimate = strain in reinforcing steel (compression side) at ultimate = strain in prestressing steel at the level of CGS at ultimate = stress in reinforcing steel (tension side) at ultimate = stress in reinforcing steel (compression side) at ultimate = stress in prestressing steel at ultimate.
p
xu s s pu fs fs fpu
The strain difference (p) is further explained in Section 3.4, Analysis of Member under Flexure (Part III).
The stress block in concrete is derived from the constitutive relationship for concrete. The relationship is explained in Section 1.6, Concrete (Part II). The compressive force in concrete can be calculated by integrating the stress block along the depth. The stress in the tendon is calculated from the constitutive relationship for prestressing steel. The relationship is explained in Section 1.7, Prestressing Steel.
Indian Institute of Technology Madras
The expressions of the forces are as follows. Cs = Asfs Cc = 0.36fckxub Tp = Apfpu Ts = Asfs The strengths of the materials are denoted by the following symbols. fck fpk fy = characteristic compressive strength of concrete = characteristic tensile strength of prestressing steel = characteristic yield stress of reinforcing steel
(3-6.1) (3-6.2) (3-6.3) (3-6.4)
Based on the principles of mechanics (as explained under the Analysis of a Rectangular Section in Section 3.4, Analysis of Member Under Flexure (Part III)), the following equations are derived.
1) Equations of equilibrium The first equation states that the resultant axial force is zero. This means that the compression and the tension in the force couple balance each other.
F = 0 Tu = Cu Tp +Ts = Cc + C' s
' ' Ap fpu + As fs = 0.36fck xu b + As fs
(3-6.5)
The second equation relates the ultimate moment capacity (MuR) with the internal couple in the force diagram. MuR = Ts ( d - d p ) + Cc ( d p - 0.42 xu ) + C' s ( d p - d' ) = As fs ( d - d p ) + 0.36fck xu b ( d p - 0.42 xu ) + A' s fs' ( d p - d' ) 2) Equations of compatibility For each layer of steel there is a compatibility equation. If there are distributed
(3-6.6)
Ap
reinforcing bars in several layers and the spacing between the layers is large, then the use of compatibility equation for each layer is more accurate than the use of one compatibility equation for the centroid of the layers. The following equations are
(3-6.7)
(3-6.8)
(3-6.9)
3) Constitutive relationships a) Concrete The constitutive relationship for concrete is considered in the expressions of Cc. This is based on the area under the design stress-strain curve for concrete under compression.
b) Prestressing steel
fpu = F1 ( pu )
c) Reinforcing steel fs = F2 ( s ) f = F3 (
' s ' s
(3-6.10)
(3-6.11) (3-6.12)
(3-6.13) (3-6.14)
The known variables in an analysis are: b, d, d, dp, As, As, Ap, p, fck, fy and fpk. The unknown quantities are: MuR, xu, s, s, pu, fs, fs and fpu. The objective of the analysis is to find out MuR, the ultimate moment capacity. The previous equations can be solved by the strain compatibility method as discussed for the fully prestressed rectangular section. 1) Assume xu. 2) Calculate pu from Eqn. 3-6.7. 3) Calculate fpu from Eqn. 3-6.10. 4) Calculate Tp from Eqn. 3-6.3. 5) Calculate s from Eqn. 3-6.8. 6) Calculate fs from Eqn. 3-6.11. 7) Calculate Ts from Eqn. 3-6.4. 8) Calculate s from Eqn. 3-6.9.
Indian Institute of Technology Madras
9) Calculate fs from Eqn. 3-6.12. 10) Calculate Cs from Eqn. 3-6.1. 11) Calculate Cc from Eqn. 3-6.2. If Eqn. 3-6.5 (Tu = Cu) is not satisfied, change xu. If Tu < Cu decrease xu. If Tu > Cu increase xu. 12) Calculate MuR from Eqn. 3-6.6. The capacity MuR can be compared with the demand under ultimate loads.
A sectional analysis is not possible. The analysis involves integrating the strain in concrete to calculate the deformation p = cp Here, p = deformation of the tendon cp = deformation of the concrete at the level of prestressing steel (CGS). The change in stress in steel (fp) at ultimate is determined from p. The stress in steel at ultimate is given by the sum of the effective prestress (fpe) and fp. fpu = fpe + fp
(3-6.16)
over
the
length
of
the
member.
The value of fpu is less than that for a bonded tendon. The ultimate moment is given by the following equation.
MuR = Ap fpu ( d - 0.42 xu )
(3-6.17)
based on the amount of prestressing steel. The later is expressed as the reinforcement index p = Apfpk / bdfck. Table 12 is reproduced as Table 3-6.1 which is applicable for
unbonded post-tensioned beams. The values of fpu and xu are given as fpu/fpe and Xu/d, respectively. The effective prestress (after the losses) in a tendon is represented as fpe. Values of xu and fpu for unbonded post-tensioned rectangular beams (Table 12, IS:1343 - 1980) fpu/fpe p 30 0.025 0.05 0.10 0.15 0.20 1.23 1.21 1.18 1.14 1.11 For values of L/d 20 1.34 1.32 1.26 1.20 1.16 10 1.45 1.45 1.45 1.36 1.27 30 0.10 0.16 0.30 0.44 0.56 xu/d For values of L/d 20 0.10 0.16 0.32 0.46 0.58 10 0.10 0.18 0.36 0.52 0.64
Table 3-6.1
The values of fpu/fpe and xu/d from Table 3-6.1 are plotted in Figures 3-6.2 and
3-6.3,
respectively. It is observed that with increase in p, fpu reduces and xu increases. This is expected because with increase in the amount and strength in the steel, the stress in steel drops and the depth of the neutral axis increases to maintain equilibrium.
1.5
l /d
fpu/fpe
30 1.25 20 10
p
Figure 3-6.2
0.6
l /d
0.4
30
20
10
xu / d
0.2 0
0.05
0.1
0.15
0.2
p
Figure 3-6.3
Thus given the value of p for a section, the values of fpu and xu can be approximately calculated from the above tables.
=
Here,
c + cp d
(3-6.18)
c = extreme concrete compressive strain cp = strain in concrete at the level of prestressing steel (CGS) d = depth of the CGS. The following sketch shows the curvature () in the strain profile.
d Ap
cp Cross-section
Figure 3-6.4
Strain profile
Definition of curvature
The analysis of behaviour involves the following three principles of mechanics. 1) Equilibrium of internal forces with the external loads at any point of the behaviour. There are two equilibrium equations. a) Force equilibrium equation b) Moment equilibrium equation. The internal forces in concrete and steel are evaluated based on the respective strains, cross-sectional areas and the constitutive relationships.
2) Compatibility of the strains in concrete and in steel for bonded tendons. This assumes a perfect bond between the two materials. For unbonded tendons, the compatibility is in terms of deformation.
3) Constitutive relationships relating the stresses and the strains in the materials. The relationships are developed based on the material properties.
The equilibrium and compatibility equations and the constitutive relationships can be solved to develop the moment versus curvature curve for a section.
The following plot shows the curves for a prestressed section and a non-prestressed section. The two sections are equivalent in their ultimate flexural strengths.
Figure 3-6.5
From the previous plot, the following can be inferred. 1) Prestressing increases the cracking load. This leads to the following benefits.
For the prestressed member, there is a negative curvature causing camber in absence of external moment.
4) For a given reverse moment, the curvature of the prestressed member is larger.
6) For a partially prestressed section with the same ultimate strength, the moment versus curvature curve will lie in between the curves for prestressed and non-prestressed sections.
Ductility
The ductility is a measure of energy absorption. For beams, the curvature ductility () is defined as
=
Here, u = curvature at ultimate y = curvature at yield.
u y
(3-6.19)
For prestressed beams, y can be defined corresponding to a plastic strain of 0.002 in the prestressing tendons. It has been observed that the ductility of prestressed beams is less than that in reinforced concrete beams.
In design of members for seismic forces, ductility is an important requirement. In addition, seismic forces lead to reversal of moments near the supports of beams in a moment resisting frame. Hence, prestressing of beams in a moment resisting frame is not recommended in seismic areas.
Experimental Investigation
The behaviour of a beam and its ultimate strength can be determined by testing prototype specimens. The tests can be conducted under static or dynamic loads. Testing also helps to check the performance of the anchorage units.
The following photo shows the set-up for testing a prototype bridge girder.
Figure 3-6.6